After 10 years of good service, I encountered the problem with filament clogging the teflon tube near heat-break area.
Because all worked more/less without problems for a long time, I am puzzled this problem surfaced now.. obviously some setting was too close to wrong value and possibly change of the environmental temperature tipped the scale in wrong direction..
Printer is DIY, with MK-8 print head (one extruder), and I am using ABS (bed 100°C, hot end at 240°C).
Is there some setting in EEPROM that can help mitigating this problem?
Thank you in advance for any reply/suggestion!
Bojan